Suzhou Xunshi New Material Co., Ltd

SUZHOU XUNSHI NEW MATERIAL CO., LTD CHOOSE XUNSHI, CHOOSE HIGH PERFORMANCE

Manufacturer from China
Verified Supplier
8 Years
Home / Products / Permanent Magnet Alloy /

0.05~3.0mm Permanent Magnet Alloy Cold Rolled Strip For Recording Material 2J33

Contact Now
Suzhou Xunshi New Material Co., Ltd
Visit Website
Province/State:jiangsu
Country/Region:china
Contact Person:MrAllen Sun
Contact Now

0.05~3.0mm Permanent Magnet Alloy Cold Rolled Strip For Recording Material 2J33

Ask Latest Price
Video Channel
Brand Name :XUNSHI
Model Number :2J33
Certification :ISO 9001:2015
Place of Origin :China
MOQ :30kg
Price :Negotiable
Payment Terms :T/T
Supply Ability :200 kg per week
Delivery Time :45-50 days
Packaging Details :Plywood case
Spec :GB/T 14989-2015
Diameter :0.05~3.0mm
Forms of supply :Cold drawn wire, cold rolled strip
Hc :27.86 kA/m
Br :0.60 T
Br·Hc :18.31 kJ/m3
more
Contact Now

Add to Cart

Find Similar Videos
View Product Description

2J33 Permanent-Magnet Alloy Cold Rolled Strip for Recording Material

A-ONE ALLOY is able to produce 2J33 permenent magnet alloy in forms of wire, strip or per customer requirement.

2J33 is used to make small section permanent magnet and recording material.

Forms available: cold drawn wire and cold rolled strip

Size range:

Wire diameter: 0.05~3.0mm

Strip thickness: 0.20~1.00mm

Chemical composition

Element C Si Mn P S Ni Co V Fe
Weight(%) 0.12 max. 0.50 max. 0.50 max. 0.025 max. 0.020 max 0.70 max. 51.0~53.0 11.8~12.7 Balance

Delivery condition: without heat treatment

The parts should be heat treated after they are processed to get required magnetic properties.

Magnetic properties(after heat treatment)

Form Cold drawn wire Cold rolled strip
Parameter

Hc

(kA/m)

Br

(T)

Br·Hc

(kJ/m3)

Hc

(kA/m)

Br

(T)

Br·Hc

(kJ/m3)

Value 31.84 min. 0.70 min. 23.88 min. 27.86 min. 0.60 min. 18.31 min.

Heat treatment

Grade Temperature(°C) Duration(min) Cooling
2J33 580~640 20~60 air cool